Professional manufacturer of tile grout and adhesives with 27 years experience.

[Beauty Glue Construction] Standardized Construction Process of Real Porcelain Glue-Beauty Glue Factory

by:Kastar     2021-04-06

The tutorial videos of the beauty joint agent construction on the Internet are mostly the construction process of the one-component beauty joint agent, and the two-component real porcelain glue construction tutorial is also non-standardized. The following is a detailed analysis of the beauty joint agent factory crystal porcelain king Standardized construction process of real porcelain glue. Tools required for construction: gloves, tile cleaning wax, seam cleaning tools, utility knife, Yin and Yang angle scraper, pressure seam steel ball, spatula, two-component glue gun, vacuum cleaner, etc. Pre-construction preparations: Put on gloves, use seam cleaning tools, utility knives, etc. with a vacuum cleaner to clean up the construction waste in the gaps between tiles. In order to protect the tiles, please evenly apply the special tile cleaning wax from the Meijiao factory to the surface of the tiles on both sides of the tile gaps, and be careful not to rub them into the gaps. , Unscrew the product bottle cap, squat the product on the ground a few times to exhaust the air in the bottle. Press and hold the glue gun pressure relief button, and pull out the push rod. Put the Jingci Wangmei seam agent product into the glue gun. The groove at the shoulder of the bottle should be inserted into the glue gun head to prevent the bottle body from bursting due to uneven force during construction. , Press the glue gun without the mixing tube, until the two tubes are discharged at the same time. Then install a special mixing rod, and use a utility knife to cut out a suitable glue outlet according to the width of the brick gap. Discard the unmixed materials about a centimeter from the front end. After the glue is finished, press the pressure relief button of the glue gun to stop the glue. Formal construction: During construction, the glue outlet is aligned with the tile gap, and the material is uniformly driven into the gap at a uniform speed, and a short section is punched out to both sides at the intersection. This method is for beginners to press the seam later. , Use pressure seam steel balls to flatten the material, and press the intersection to both sides. , The construction in other directions is the same, until all the gaps are filled. , When the female corner is beautifully stitched, the material should not be too much so as not to affect the pressure seam. It is recommended to use small pressure seam steel balls for pressure seam. 、When the external angle is beautifully stitched, more material can be used to facilitate the pressing. It is recommended to use the external angle scraper to press the sewing. Follow-up work: The finished seam must be allowed to stand for hours, depending on the temperature, the lower the temperature, the longer the time. , After the material is solidified, shovel the remaining material away with a US sewing shovel. , Leave it to cure for hours. Note: Please use the glue gun specified by the Meijiao factory, otherwise the pressure will be uneven, resulting in product piston rupture or partial non-curing of the Meijiao. , Long-distance transportation will cause air in the product bottle. Please open the bottle cap and squat a few times before use, and then push the piston with the glue gun until the two tubes are discharged at the same time before installing the mixing rod for construction to prevent glue breaking during the construction process. Air bubbles or partial non-solidification caused by uneven mixing of materials. , Every time you use a new mixing rod, be sure to throw out about centimeters of the front end of the material and discard it to prevent local uncured phenomenon caused by uneven mixing of materials. , When gluing, the groove at the shoulder of the product bottle should be embedded in the glue gun tip, and the bottle body should be supported by hand to prevent the bottle body from bursting due to uneven force during construction. , The construction environment must be clean and dry, whether the product will change color or adhesive force will drop, cracking and other problems. , Try to avoid using the light-colored beautifying agent outdoors. The ultraviolet rays in the sun will accelerate the discoloration and aging of the beautifying agent. , When the temperature is lower than ℃, the viscosity of the epoxy resin will increase, making the material difficult to beat. Please use -℃ water to heat it for one minute before use.
Beauty Glue Beauty Glue Factory Construction Real Porcelain Glue
Custom message
Chat Online 编辑模式下无法使用
Leave Your Message inputting...