US joint agent construction method and construction precautions!



Question: For beautiful seams, what is the most suitable gap when laying tiles?



Answer: There is no fixed value for the gap width of the tiles. If you consider the effect and cost of the beautiful seams, it is generally recommended to be a -mm seam width. This width not only satisfies the beautification effect of the tile gaps , It is also considered for its personal cost. Of course, if the cost is not considered, the slit width of mm is the best embodiment of the slit effect of the beautiful slit.



Question: Is it necessary to use a grout as a primer for the beautiful joints of ceramic tiles?



Answer: Generally, it is advisable to use a sealant as a primer and leave a seam depth of about mm, so as to consider the cost and maintain a good use time. If you do not consider the cost factor, you do not need the sealant as the primer. Its adhesion is maintained for a longer period of time.



Question: Is the construction of two-component beauty joint agent scraped with a scraper? Or use the sewing ball to press it?



Answer: If you use a scraper to scrape, then after the scraper is finished, the beautifying agent and the gap will be flat. In this way, the scratching in daily life is unavoidable, and the accumulation of time will easily cause the gloss to decrease. If you use a press ball, there will be micro grooves in the gap to prevent scratching in daily life.



Question: Before making beautiful seams, can the sealant be used if it is found to be wet?



Answer: No. Because if the caulk is wet, its water vapor evaporates and penetrates into the caulking agent, changing the molecular structure of the caulking agent, especially the two-component caulking agent. The water vapor will make the curing agent ineffective. If it is in the bathroom, because The lower layer is waterproof. The last time the beautifier is also waterproof, it will cause the beautifier to top out, so be sure to keep the grout dry and the gap dry. To have perfect results.



Question: Is the higher the hardness of the two-component beauty joint agent, the better?



A: The hardness is not the harder the better. It must be soft and rigid, like iron wire, not only has the hardness of iron, but also has good toughness.



Question: After the two-component beautifying agent is applied, some places do not dry, how long will it take?



Answer: If there is still part of the two-component beautifying agent that does not dry after an hour, the main reason is that the epoxy resin and the curing agent are not completely mixed, resulting in no drying. Generally, there is no need to wait. Because it is impossible to dry any more in this situation, you can only buckle up the non-dried ones and re-apply. This is a normal phenomenon of two-component beauty joint agent. It is recommended not to finish the construction at one time and leave some remaining materials repair.