Professional manufacturer of tile grout and adhesives with 20 years experience.

Does the bubble bulging of the beauty joint have any effect? What causes it? How to deal with it? -Beautiful seam agent factory

by:Kastar     2021-04-06

It has become a common phenomenon to use beauty joints to decorate ceramic tiles in home decoration. The beauty joint construction technology has been relatively mature, but there are still various problems. Today, the editor saw a few messages asking, does the bubble bulging of the beauty joint matter affect it? What causes it? How to deal with it? The editor also consulted many professional seamstresses, and finally summarized a few possible causes and solutions for bubble bulging for your reference. 1. Air is mixed in during the production and transportation of products. During the production process, some raw materials need to be mixed and stirred. It is inevitable that air will be mixed in. The regular beauty grout manufacturers will vacuumize before filling, in order to let the mixed air out of the material. To avoid affecting the construction and use. Informal manufacturers may omit this step in order to save costs, so bubbles and bulges will appear during construction. A small part of the air will be mixed in due to the bumps during the logistics and transportation, and the air discharged before the beautiful seam construction will not affect the use. Solution: The user should exhaust the beauty joint agent before the beauty joint construction. First unscrew the cap of the beauty joint agent bottle, use the glue gun to push the two tubes of material until the two tubes are glued at the same time, then screw on the mixing nozzle, and after the front end is not evenly mixed, the normal beauty stitching can be constructed. 2. The base layer is not properly treated. There is dust or water vapor in the cracks of the tiles. Just after the tiles are laid, the base layer will be relatively damp, and the water will evaporate to form water vapor and cause bubbles to bulge in the beautiful seams. Even if the base layer is completely dry, there will still be cement mortar particles and dust in the cracks of the tiles, causing the glue to be uneven. Solution: After the tiles are laid, ventilate and dry for about a week. If you encounter rainy days, you need to close the doors and windows and extend the drying time appropriately. If possible, you can turn on floor heating or air conditioning to shorten the drying time. Before the US joint construction, use a joint cleaning tool and a vacuum cleaner to clean the tile gaps. 3. The opening of the mixing glue nozzle is too large and the glue speed is too fast. Because the opening of the mixing glue nozzle is too large, the glue is too thin after quick glue, and can only be attached to the surface of the tile joints. After the pressure seam, there will be a bulging situation. Solution: The opening of the mixing glue nozzle should be smaller than the tile gap, and the glue nozzle should be perpendicular to the gap. Glue at low speed, so that the beauty grout can fully enter the tile gap and eliminate the air in the gap. If you still encounter air bubbles when pressing the seam, you can break the air bubbles, make up some beautifying agent, and re-compact the seam. Fourth, the heating temperature of the beautifying agent is too high. The fluidity of the beautifying agent in winter will be reduced, and the construction will be somewhat difficult. In order to soften the beautifying agent and reduce the difficulty of gluing, heating is often used to solve the problem. If the heating temperature is too high, there will be a large temperature difference with the construction environment, which will cause water vapor to accumulate and cause bubbles to be generated. Solution: When the beauty seam agent is heated, the temperature can be controlled between -℃. It is recommended to use a constant temperature electric heating package. If it is heated with water, dry the bottle before use to prevent water from being mixed in. Under normal circumstances, there may be more than one reason for the bubble bulging of the beauty joint agent, and it may be caused by a variety of factors. Strictly operating in accordance with the beauty joint construction specification can greatly reduce the occurrence of bubble bulging.
Beauty Seam Agent Causes Air Bubbles Treatment Bulge
Custom message
Chat Online 编辑模式下无法使用
Leave Your Message inputting...