Floor paint construction process is analysed, five standard processes share
on the finishing materials, lightsome coating, ceramic tile instead of the clunky, has become an irreversible trend. Except on the outer wall material, the government introduced gradually forced to disable the ceramic tile, stone implement paint to paint the walls, some large public space ground adornment widely used are coatings in terms of building materials & ndash; — Floor paint and so on, thus formed and a new field of coating demand rapid growth. A good floor paint project, cannot leave the construction process of a specification, specific as follows & ndash; —
1, the element with
(1) basic element to smooth or stone for the cement powder;
(2) the ground need to preserve one's health more than 28 days, the water should be below 8% before the construction element to any grievances or empty drum need to be removed;
3. Fill with mortar ground;
element (4) to the oil pollution should be thoroughly cleaned;
5. Before the construction needs to keep the construction element of dry and clean; Polished away
6 loose bed, delaminating and cement residue, hard, smooth, and increase the floor coating adhesion with the ground.
1. 2, bottom coating construction needs to keep clean if there are any sundry adhesive to be cleared before, according to the correct proportion mixing main agent and curing agent, mixing fully;
(2) must be completed according to the condition of the ground to adjust the proper viscosity mixed materials must be completed within 4 hours and construction;
3. Bottom coating curing hardening time about 8 hours or more;
(4) the floor after closed primer with good water, brush, roller coating, coating, or make it fully wetting concrete, and seep into the concrete lining.
3, the coating (1) before the construction need to clean debris adhesion to remove, if any, in accordance with the correct proportion mixing main agent and curing agent, mixing fully;
(2) will be completed mixed resin to join a moderate amount of quartz sand;
(3) using trowel materials evenly coated;
(4) mixed complete material construction within 30 minutes;
5) construction junction disposal of the transition;
6 coating curing hardening time in about eight hours or more;
7) will be in the coating materials mixed with just the right amount of quartz sand fully stir well, with a trowel trowel painted leveling &compaction layer of certain thickness.
4, batch of soil (1) in accordance with the correct proportion mixing main agent and curing agent, mixing fully;
(2) the use of knife material coated uniformly;
3. Mix complete construction materials need 30 minutes;
(4) of soil health hardening time about 8 hours or more;
5. Depending on the actual needs of construction demand level and no holes, no batch of knife is printed and sanding shall prevail.
6 using surface coating material with quartz powder coating, besmear fill in the gaps between the larger particles, after being cured, with a clean machine polishing surface, use a vacuum cleaner to suck the dust and sand.
5, surface coating (1) the construction needs to keep clean if there are any sundry adhesive to be cleared before;
2. The main agent before use mix;
(3) in accordance with the correct proportion mixing main agent and curing agent, mixing fully;
(4) use roller or trowel mix material evenly coated finish materials to the construction completion within 30 minutes;
5) construction junction to disposal of the transition;
6. After completion of construction, can be stepped back for 24 hours, 72 hours rear can weight ( Will be subject to 250 c, low temperature should be moderately open) 。