Floor paint construction of large inventory
with high-speed development of Chinese economy and the construction industry and to increasing demand for floor paint, and then promote the floor paint in the prosperous period. Floor lacquer is bright beautiful, practical, beautiful, wear resistance, waterproof, anti-corrosion and other characteristics, widely used in workshop, parking lot, playground and other places. However handled properly in the construction will present all sorts of questions, small make up inventory floor paint with you during the construction of the present all kinds of questions.
1, the floor bleeding doubt
bleeding is to point to in a film on the lacquer of another kind of color coated, the underlying some into the surface coating and makes the appearance of coating color on the surface. The no. 1 is the cause of the bleeding: primer, primers and paint color difference, we do not besmear bottom or substrate containing color material, primer containing organic pigments.
2, floor paint, paint hair flower doubt
refers to the coating appearance some uneven color, render spot mark, stripes and hue disheveled appearance, reason first is due to the construction process, construction paint is not abundant mixing evenly, alter the uneven and coating composition change, etc.
3, white floor paint appearance question
refers to the construction work is completed, the surface coating of altered white appearance, cause there are a few points: high humidity in the air may be low temperature, frost, water vapor on the coating composition of curing agent and amine separated, white mist rally in appearance.
4, floor paint, wrinkling fisheye doubt
wrinkle is in the process of coating boring because of the difference between surface layer and the surface dry speed dramatically shorten tucked up make the coating appearance presents wrinkles uneven or random linear representation; Fisheye is some coating after coating construction be exist or mixed with paint of paint looks foreign body affected uneven coating adhesion is shrunk and reveal the coated surface appearance; Paint after coating is sharply due to solvent evaporation to the lacquer liquid supplement, constitute a lot round circle or like leather pores needle puncture of the appearance of
5, floor paint, wrinkling, have pinhole questions
coating surface wrinkling appearance, first reason is to paint inside and outside to consolidate boring speed inconsistent constitute a layer of surface layer peeling, pinhole is due to the curing agent is mixed with paint, in the coating occurred by mixing a large number of bubbles, bubbles in the process of curing escape, leave a mark in the film and become a pinhole.
6 holes, floor paint, craters doubt
the base surface uneven density or packing of lack will cause the ground like a non-stick oil present circular hole, hole we called craters. Solution is must be carefully check before construction base, have a question that needs careful handling, and then to construction epoxy floor paint. Choose packing with good sex of wandering, and strengthen the management of data quality.
7, floor paint, rough, cracking question
the rough surface is refers to the surface with intrusive different granular material, the primary reason is not easy to dissolve impurities in floor coating and outside caused by dust. Surface crack appearance is due to the original data and construction quality question, the paint adhesion force is reduced, under the external force, present the appearance of peel cracking.
8 and the fullness of the floor paint drop grinning bad doubt
drop is due to the floor cracking lost the original adhesion to substrate under the action of external force, the film into small some or the entire jie skin from the surface of the material: grinning and question of fullness not mostly the original data and construction. Always epoxy floor paint to make must choose good materials and professional construction team with professional quality can be ensured.
9, floor paint curing slow
is slow curing epoxy resin material at exceptionally low temperature ( 10° C) Slow curing reaction. 5° C is sure to stop the construction. Has a strong link that appearance and viscosity, the lower the temperature, the higher the viscosity will be, then it will be hard. Curing time is too long would amount to a coating with dust, sand and other stolen goods, and even slow down the time limit for a project. Still is in the construction site and solvent will constitute a curing slow, due to the evaporation of the solvent will take away some of the heat and cooling coating.