The seam an agent after construction, there are part owner will find no curing, is what we call curing incomplete, this is what causes? Beautiful seam an agent factory beautiful seam an agent small make up today with everyone together to get to know the reason.
the seam an agent without good curing to do
the reason one: the seam an agent has been sunshine point-blank, causing viscosity damage. The seam an agent containing epoxy resin raw materials, the material determines its under high temperature is not allowed. If direct sunlight exposure, or otherwise in temperature higher carriage frowsty, viscous bad problems will appear. In addition, the seam an agent is double group, two groups of different performance, if because of the above problems, lead to two groups of mixing ratio not harmonious, curing incomplete phenomenon will occur. As a result, the seam an agent storage must pay attention to.
the reason two: glue guns quality closes nevertheless, or too serious wear and tear, and the secondary glue is uneven. On the market for the sale of some of the glue guns, there is no guarantee quality, use process will often appear the details, there are some glue guns, quality guaranteed, but the using time is longer, more serious wear and tear, such glue guns connecting rod core shift. Once the core shift, hose uneven, group A beautiful seam an agent reflow fast and fierce, group B return slow and gentle beauty seam an agent, the both uneven, also can appear curing is not comprehensive. So, choose the glue guns to choice of glue gun, or directly with the electric gun, if use for long time, pay attention to the maintenance in place.
the reason 3: using a new product, not according to the requirements of heading discarded waste. We have emphasized for everyone, in open bottle caps, edging out part of the first, until 2 tube discharge at the same time, and then mount mixing tube, 30 cm length of the seam an agent, to construction, because the product at the time of filling, machinery and equipment limited, there may be some error in order to achieve a 1:1 ratio, must be discarded. Some friend did not do a good job in this step, so the proportion is wrong, also caused the part without curing. So, when use, everybody must come as required.
reason four: the problem of mixing tube, spiral pipe have burrs in mixing tube, or the small size, results in uneven material is very close, it is the leading cause of curing incomplete possible factors.
the above is the seam an agent without curing good main reason, friends to suit the remedy to the case, please!